皮皮虎 发表于 2011-8-5 01:27

关于PCB板虚焊的实验

不知现在有没有相应的实验标准,专门用于考核电路板的虚焊这一块,请教。

cwladt 发表于 2011-8-5 08:11

有,你是打算找实验室做实验还是找试验标准?

皮皮虎 发表于 2011-8-6 21:09

回复 2 # cwladt 的帖子

我想先看看标准标,再决定做试验

cwladt 发表于 2011-8-8 22:25

你给留联系方式?我联系你

szdlliuzm 发表于 2011-8-8 22:59

这样的试验条件是很好设置的,用正弦试验就是10-300Hz或10-500Hz,定加速度2-5g, 如果是机械振动台就定振幅,10-55Hz,定振幅0.75mm.
也可以是随机振动,10-300(500)Hz,平直谱,均方根加速度2-5g,

szdlliuzm 发表于 2011-8-8 23:00

如果是要做破坏性试验,提高加速度值就可以了。

皮皮虎 发表于 2011-8-9 07:08

回复 6 # szdlliuzm 的帖子

是什么标准?

Jonah_K500 发表于 2011-8-9 09:00

回复 1 # 皮皮虎 的帖子

JEDEC Specifications
1. JESD22-B108-A “Coplanarity Test for Surface-Mount Semiconductor Devices”, Jan., 2003.
2. JESD22-B103-B “Vibration, Variable Frequency”, June, 2002.
3. JESD22-A104-B “Temperature Cycling”, July, 2000.
4. JESD22-B104-B “Mechanical Shock”, March, 2001.
5. JESD22-A113-D, “Preconditioning of Non-Hermetic Surface Mount Devices Prior to Reliability Testing”, August 2003
6. J-STD-002B “Solderability Tests for Component leads, Terminations, Lugs, Terminals, and Wires”, February 2003.
7. J-STD-020C “Moisture / Reflow Sensitivity Classification for Non-Hermitic Solid State Surface Mount Devices”, July 2004
8. J-STD-033a “Standard for Handling, Packing, shipping and Use of Moisture/Reflow Sensitive Surface Mount Devices
9. J-STD-035 “Acoustic Microscopy for Nonhermetic Encapsulated Electronic Components
10. EIAJED-4701/301A “Resistance to Soldering Heat for Surface Mount Devices (SMD), Test Method 301A

IPC Specifications
1. IPC-A-610D, “Acceptability of Electronic Assemblies”, January 2000
3. IPC-SM-785 “Guidelines for Accelerated reliability Testing of Surface Mount Solder Attachments.”, November 1992
3. IPC-TM-650 “IPC Test Methods Manual”
4. IPC-9701 “Performance Test Methods and Qualification Requirements for Surface Mount Solder Attachment”, January 2002

MIL Specifications
1. MIL-STD-202G, Method 210F “Resistance to Soldering Heat”, February 2002.Must meet modified test conditions according to Dell requirement and Lead Free solder used.

皮皮虎 发表于 2011-8-16 21:28

非常感谢!

atomjin 发表于 2011-9-21 18:12

脚丫子真能踩,厉害!

huzilong 发表于 2011-9-21 21:29

{:{40}:}

xiaohengjj 发表于 2011-9-23 11:55

回复 8 # Jonah_K500 的帖子

丫的,整那么多出来,够猛!